文献和实验Preparing Colloidal Gold for Electron Microscopy
after they have been made. To make 100 ml of gold sol, two stock solutions have to be prepared. Solution A 80 ml distilled water and 1 ml 1% aqueous gold chloride. Solution B 4 ml 1% tri
Preparing Colloidal Gold for Electron Microscopy
these particles to protein A and how to purify the probes after they have been made. To make 100 ml of gold sol, two stock solutions have to be prepared. Solution A 80 ml distilled water and 1 ml 1% aqueous gold chloride. Solution B
【共享】Present and future applications of gold in rapid assays
), have employed gold nanoparticles as the label of choice. Particle Size. Gold nanoparticles used in lateral-flow tests are smaller than latex. The size of the pores in the test’s nitrocellulose membrane is 8–10 µm, enabling many nanoparticles